Products
Carbon Steel Continuous Pickling Unit (CPL)
Classification Solution
The continuous hydrochloric acid pickling process is adopted to remove the iron oxide layer on the surface of the hot-rolled steel strip and cut off the irregular edges of the steel strip to provide qualified hot-rolled steel materials for the next process. The steel strip after pickling has a pure iron surface and can be cold rolled or hot-dipped galvanized.
- Overview
- Inquiry
- Related Products
The continuous hydrochloric acid pickling process is adopted to remove the iron oxide layer on the surface of the hot-rolled steel strip and cut off the irregular edges of the steel strip to provide qualified hot-rolled steel materials for the next process. The steel strip after pickling has a pure iron surface and can be cold rolled or hot-dipped galvanized.
Unit characteristics
Continuous pickling unit, with automatic argon arc welding machine and Polin pull straightening machine at the entrance, hydrochloric acid multi-stage shallow groove turbulent pickling process and multi-stage water rinsing process in the process section, disc cutter and electrostatic oiling machine at the outlet section Wait.
Annual production scale: 800,000-1,200,000t/a
Raw material: Carbon steel hot rolled coil
Steel grade: CQ, DQ, DDQ, IF, HSLA, W440-W1300 silicon steel
Raw material specifications: 1.5-6.0mmx width: 650-1650mm
Roll diameter: I.D.Φ760/Φ610mmO.D.MaxΦ2150mm Maximum roll weight: 30t
Hot rolled coiling temperature: Max670 degrees (IF<720 degrees)
Process speed: Max150mpm
Pickling time: 25-30sec
adopt SIEMENS or ABB electrical control system
Production process

Rolling→Uncoiling→Cut-heading→Welding→Entry Looper→Po Lin-Straightening→Pickling→Water Rinsing→Drying→Export Looper→Cutting Edge→Greasing-Splitting Cut→Reel->Unload→Package
EN
AR
FR
DE
EL
HI
IT
JA
KO
NO
PL
PT
RO
RU
ES
TL
ID
UK
VI
HU
TH
TR
FA
AF
MS
BE
UR
BN
JW
LA
MI
MN
NE
PA
KK
TG
UZ
KY